N2 - (Fe100-xBx)0.89N11 (at. %) films with x = 18 and 25 are formed on thermally oxidized Si substrates at room temperature and then annealed at 200 °C or 400 °C. The influences of annealing on the microstructural, electrical, magnetic, and magnetostrictive properties are investigated. Granular structure is realized in the films both without and with annealing, where Fe-B-N grains of about d = 5 nm diameter are surrounded by boundaries consisting of amorphous B-N phase. The grains are composed of an amorphous phase for the films without and with annealing at 200 °C. On the other hand, parts of the grains are crystallized and tend to coalesce together by annealing at 400 °C. Furthermore, formation of the B-N phase is enhanced by employing a B-richer content of x = 25 and a higher annealing temperature of 400 °C. The Fe-B-N films without and with annealing exhibit high electrical resistivities of ρ = 230-1550 μΩcm, when compared with the cases of nanocrystalline materials such as Fe-B-Si-Nb-Cu and Fe-B-Si-P-Cu. However, by annealing at 400 °C, the resistivities of films with x = 18 and 25, respectively, decrease from ρ = 500 to 230 μΩcm and from ρ = 1550 to 930 μΩcm due to the partial coalescence of grains. By contrast, the saturation magnetizations of films with x = 18 and 25 are, respectively, improved from Ms = 0.9 to 1.2 kemu/cm3 and from Ms = 0.5 to 0.8 kemu/cm3, possibly because the Fe content in grains increases through the segregation of B and N atoms to the grain boundaries. Moreover, the saturation magnetostrictions of films with x = 18 and 25 are, respectively, suppressed from λs = 21 × 10-6 to 3 × 10-6 and from λs=9 × 10-6 to 5 × 10-6 due to the partial crystallization of grains and/or due to the variation of the B and N contents within the grains. The present study has shown that granular Fe-B-N alloy is one of the candidates for soft magnetic materials with high resistivity and low magnetostriction.
AB - (Fe100-xBx)0.89N11 (at. %) films with x = 18 and 25 are formed on thermally oxidized Si substrates at room temperature and then annealed at 200 °C or 400 °C. The influences of annealing on the microstructural, electrical, magnetic, and magnetostrictive properties are investigated. Granular structure is realized in the films both without and with annealing, where Fe-B-N grains of about d = 5 nm diameter are surrounded by boundaries consisting of amorphous B-N phase. The grains are composed of an amorphous phase for the films without and with annealing at 200 °C. On the other hand, parts of the grains are crystallized and tend to coalesce together by annealing at 400 °C. Furthermore, formation of the B-N phase is enhanced by employing a B-richer content of x = 25 and a higher annealing temperature of 400 °C. The Fe-B-N films without and with annealing exhibit high electrical resistivities of ρ = 230-1550 μΩcm, when compared with the cases of nanocrystalline materials such as Fe-B-Si-Nb-Cu and Fe-B-Si-P-Cu. However, by annealing at 400 °C, the resistivities of films with x = 18 and 25, respectively, decrease from ρ = 500 to 230 μΩcm and from ρ = 1550 to 930 μΩcm due to the partial coalescence of grains. By contrast, the saturation magnetizations of films with x = 18 and 25 are, respectively, improved from Ms = 0.9 to 1.2 kemu/cm3 and from Ms = 0.5 to 0.8 kemu/cm3, possibly because the Fe content in grains increases through the segregation of B and N atoms to the grain boundaries. Moreover, the saturation magnetostrictions of films with x = 18 and 25 are, respectively, suppressed from λs = 21 × 10-6 to 3 × 10-6 and from λs=9 × 10-6 to 5 × 10-6 due to the partial crystallization of grains and/or due to the variation of the B and N contents within the grains. The present study has shown that granular Fe-B-N alloy is one of the candidates for soft magnetic materials with high resistivity and low magnetostriction.
KW - Fe-B-N alloy
KW - granular structure
KW - high electrical resistivity
KW - low magnetostriction
KW - thin film
UR - https://www.scopus.com/pages/publications/105040246382
U2 - 10.1109/TMAG.2026.3696450
DO - 10.1109/TMAG.2026.3696450
M3 - Article
AN - SCOPUS:105040246382
SN - 0018-9464
VL - 62
JO - IEEE Transactions on Magnetics
JF - IEEE Transactions on Magnetics
IS - 10
M1 - 2002405
ER -